【 Solution 】 Heat transfer vinyl decoration not firm cause analysis

by:Senxi      2021-01-18
【 Solution 】 Heat transfer vinyl decoration not firm cause analysis. Heat transfer vinyl stamping rickety problems may lead to washing fastness and washing resistance heat transfer vinyl quality decline. Below for everyone to analyze thermal transfer vinyl stamping not firm problem, from the human factor and the two aspects of product quality. 1 a, human reason. Select heat transfer vinyl error. 1) Different heat transfer vinyl applications on different bearing iron content above, such as PVC ( Q6- 1) Heat transfer vinyl is mainly used on pure cotton fabric, and the sublimation heat transfer vinyl is mainly used in polyester dye sublimation cloth, TPU elastic heat transfer vinyl is mainly used in cotton, polyester, such as fiber material, selection of heat transfer vinyl error affects the effect of hot stamping. 2) Different patterns to choose different heat transfer vinyl, TPU elastic heat transfer vinyl, for example, from the type of substrate elastic heat transfer vinyl is suitable for the design of large-area Numbers, letters and patterns, and the flexibility of glue substrate heat transfer vinyl is suitable for fine pattern, Numbers and letters. 2. Parameter error in the stamping operation. The three principles: hot stamping temperature, time and pressure. Should first understand what to buy before hot stamping technology parameters of the heat transfer vinyl, TPU elastic heat transfer vinyl and thermosetting PVC heat transfer vinyl, TPU elastic printing heat transfer vinyl hot stamping temperature is 150 ℃, 10 s, and thermosetting PVC heat transfer vinyl hot stamping temperature is 170 ℃, 15 s, if thermosetting PVC heat transfer vinyl with a temperature of 150 ℃, 10 s hot stamping, so hot solid PVC heat transfer vinyl turn hot effect is not ideal, may not be strong. Two, you get what you pay for the quality of product, clear heat transfer vinyl products stamping rickety eliminate human factors, so the most likely cause of problem is heat transfer vinyl products quality problem. Heat transfer vinyl hot melt adhesive ( Glue layer) Quality instability will appear hot stamping not firm to become warped edge wrinkling problem. Sen the sunrise heat transfer vinyl factory focus on the heat transfer heat transfer vinyl, 20 years in U. S. imports of hot melt adhesive and the production of heat transfer vinyl is after high temperature hot stamping deformation, not degum, do not fade, the characteristics of high cover; With a professional attitude to provide high-quality products, services and solutions to problems. Learn more thermal transfer thermal transfer vinyl solutions to problems, or free experience heat transfer vinyl sample login, the sunrise heat transfer vinyl heat transfer vinyl factory site or call 15359509866 ( WeChat with Numbers) ! ( Above article is the sunrise heat transfer vinyl factory original, 20 years thermal transfer materials manufacturers, reprint please indicate the source! )
Custom message
Chat Online
Chat Online
Chat Online inputting...